1. … remplaçables sont montés sur un tambour en acier moulé pour plus de durabilité et une meilleure traction.   … Euroweld - RedRock Column & …
  2. … pour être utilisé dans toutes les positions et applications de soudure orbitale. Une limite d'élasticité d'au moins 610 N/mm2 à l'état …
  3. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Grey Cast Iron, …
  4. … flame welding with extreme good flowing properties without spatters during welding. Excelent mechanical strenght due to the addition of …
  5. … in case of old layers or critical base metals.. Equivalent in SMAW: Dur 62S  … 60-64 HRc hardfacing alloy, Cement, Mineral mixing peddles, …
  6. … cooling speed it is better to keep the work peace at a low temperature during welding and hammer immediately after welding. … Spheroidal Cast …
  7. … For the best results, welding must be done in a low heat input procedure and is not recommended for multi-pass applications … 1.4512,  …
  8. … la fabrication d'une construction soudée n'est pas le cordon de soudure ; le cordon moyen ne prend qu'environ 15% du temps de travail …
  9. … from porosity due to the special shaving process and cleaning method during production. AlMg4,5Mn is one of the highest grades within the …
  10. … alloy containing Nickel for more strength and bridging capability during brazing with excellent rebuilding properties.  Flux/Paste: …