1. … compte des variables comme les pertes, le cycle de travail, le renforcement de la soudure et la hauteur de la racine. Les temps de …
  2. … and corrosion at high working temperatures upto 900°C. Crack free hard facing deposit against severe thermal shock and impact. To be used …
  3. … to 550°C. as for similarly alloyed steels, quenched and tempered for cementation and nitrating. … Typ 1Cr 0,5Mo, ISO 15608: ~5,1 1.7335, …
  4. … sea water, salts and reducing acids. The weld metal is not age hardenable and when used to join Monel K-500 it has lower strength then …
  5. … weld metal composition of 12% Chromium. These weld deposits are air-hardenable that can normally be heat-treated after welding. … 1.4000, …
  6. … buffer layer except on materials considered critical or in case of old hardfacing layers. In this Situation OA 4370, ER 100 S1 or OA MnCr is … without gas (open arc). (Also weldable under M21 mixed gas) … 54 HRc hardfacing alloy for wear resistant overlays, sand pumps, valve seats, …
  7. … de consommables de soudage augmente de jour en jour en raison de l'industrie qui construit des bâtiments plus grands et plus exigeants. …
  8. … L-Ag27 is a Very good flowing, low-melting silver hard solder for operating temperatures from -200 °C to Max. 200 °C …
  9. … to type 304, high mechanical properties and good weldability, work hardening and cold-tough to -110°C. … 19% Cr / 9% Ni / 7% Mn, ISO …
  10. … to that of Rene 41 and generally superior to Inconel 718. Age hardenable while maintaining excellent high-temperature strength and …