1. … Welding Filler Material : Magnesium filler materials that match the base metal's composition are commonly used. The filler material should …
  2. … that are organized periodically. Themes such as stainless steel, nickel, aluminum, copper, cladding and welding economics have already …
  3. … with age hardenable deposit and similar mechanical properties as the base metal. Age hardened condition: 720ºC for 8 Hours, furnace Cool …
  4. … in the first layer. A buffer layer is recommended in case of sensible base material or old layers. Weldable without protective …
  5. … superalloys. CEWELD® Alloy 263 is an age-hardenable nickel-cobalt-chromium-molybdenum alloy designed specifically to … age cracking problems common for gamma prime strengthened alloys.  … NIckel based alloys with simmilar composition as Nimonic 263 … Alloy 263 …
  6. … suited for joining high carbon steels and when welding critical mixed base metal combinations. Ideal metallurgical choice for repair welding …
  7. … resistance over an ER409 alloy. Single pass welds on light gage base metal or welds with preheat do not usually require PWHT. … 1.4000, …
  8. … interpass temperature and post weld treatment as required for the base metal. Hydrogen content: < 3 ml / 100 g weld metal. …  < 620 MPa …
  9. … Cu-Al-Ni bronze. Sound, pore free deposits on ferrous and non-ferrous base materials.       Excellent resistance to cavitations and stress …
  10. … low level of free carbon and enables the filler metal to be used with Nickel 201. The weld metal has good corrosion resistance, particularly … in alkali’s. … CEWELD® NiTi 3 is developed for welding and cladding Nickel 200 and Nickel 201. This alloy is also suited for surfacing of steel. …