1. … Lower preheat and interpass temperatures are possible, yet must be approved by practical welding tests and process qualification tests. …
  2. … The weld deposit is capable of taking a high polish. TÜV-approval down to -120°C (> 32J). … ISO 15608: 8.1  Austenit ≤ 19 % Cr , TÜV …
  3. … excellent welding properties in all positions except vertically down. Easy strike, no spatter losses. Very easy slag removal. Smooth, …
  4. … and ferrite level between 30 and 50 (FN). Excellent for use in down hand welding. Excellent against pitting and stress corrosion. The …
  5. … welding characteristics. High impact strength at sub zero temperatures down to -60 °C. Weldable with Co2 and Mixed gas. … Reh < 690 MPa Iso …
  6. … thermal shock resistance and impact values at sub zero temperatures down to -196 °C … Dissimilar welds for which the electrode are used …
  7. … MPa. Crack resistant and well suited for low-temperatures, ductility down to -50°C. Preheating, interpass temperature and post weld …
  8. … welding characteristics. High impact strength at sub zero temperatures down to -60 °C. …   Reh < 690 MPa Iso 15608: 3.2 ( 460 < Reh ≤ 690 MPa) …
  9. … CrNi steels. Heat resistant up to 350°C. Excelent toughness properties down to -196°C. Good resistance to nitric acid. … ISO 15608: 8.1 …
  10. … with more deposit) No slag losses compare to 40% loss with standard electrodes.! Low amperage offers much lower heat input! 6 mm is ideal …