1. … Mn, Ni, Cr and Mo alloyed basic electrode for welding low alloyed steels with tensile strength > 620 MPa. Crack …
  2. … Without slag. Extremely crack resistant. Suitable for economic welding of CrMoV-steels up to 550 °C. Due to the seamless production …
  3. … treatable. Thicker sections should be preheated (150°C) prior to welding. … G-AlSi10Mg, G-AlSi11 G-AlSi12 (Cu), G-AlSi7Mg, G-AlSi6Cu4 , …
  4. … Submerged arc welding wire for weather resistant steels such as Corten and Patinax to …
  5. … resistance above 816°C (1500°) up to 1149°F (2100°F), especially when welding on base metals of nickel-iron-chromium alloys. … Inconel alloys …
  6. … Ductile welding deposit with high conductivity and corrosion resistance. The … … Cladding steel, Grey cast iron, Copper, Copper Alloys and dissimilar welding.  Mat.n: 2.0040, 2.0060, 2.0070, 2.0076, 2.0080, 2.0090, 20100, …
  7. … at sub zero temperatures down to - 60 °C (-80°C). Excellent welding properties. Therefore, suitable for the economic processing of …
  8. … Mn, Ni, Cr and Mo alloyed basic electrode for welding low alloyed steels with yield strength > 690 MPa. Crack …
  9. … Cr and Mo-alloyed basic elektrode for welding creep resistant steels and steel casting for working …
  10. … Applicable for welding of joints and surfacings of stabilized, corrosion resistant …