1. … It is self bonding to most materials and requires minimal surface preparation. Bond strengths in excess of 9000 psi can be achieved on …
  2. … between 1024°C (1875°F) and 1052°C (1925°F) for one hour, followed by precipitation hardening between 623°C (1135°F) … Suitable for precipitation hardening stainless steel used for welding materials of …
  3. … nodigen u van harte uit contact op te nemen voor een kennismakingsgesprek. … Dealer worden …
  4. … appearance and outstanding welding properties on both AC and DC+. Preheating is not required. … Slag crushers, Sugar cane knives, …
  5. … exhibits outstanding resistance to pitting and crevice attack in the presence of chlorides and other halides. … Alloy C-2000, 2.4675, …
  6. … resistance and good resistance to carburization and oxidation. No preheating or post heat treatment is necessary. Pay attention to low …
  7. … Seamless flux-cored wires represent a remarkable innovation in the field of welding, particularly …
  8. … 25Cr type duplex stainless steels especially for Super Duplex grade, PRE (Pitting Resistance Equivalent) is over 40. Ar-CO2 mixed gas or …
  9. … AC and DC+ with a recovery of 200% for excellent deposit performance. (Preheating is not required)Equivalent in FCAW: OA 59, OA 60 Mo, OA 61, …
  10. … at higher temperatures up to 550ºC. To much layers should be avoided, preheat is necessary to avoid cracking. A buffer layer with AA M690 or …