1. … as permanent stress by heat influence, metal wear and high surface pressure  … 1.4317, 1.4313, 1.4407, 1.4414,    GX4CrNi13-4, …
  2. … in case off multi-layer welding. The weld metal will show no undercut !Preheating is normally done to slow down the cooling speed, in case you …
  3. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150 °C), prior to welding. … Al99,0 Al.99,5 Al.99,7 E-Al., …
  4. … resistance and good resistance to carburization and oxidation. No preheating or post heat treatment is necessary. Pay attention to low …
  5. … recovery type for economic production of creep resistant steels and pressure-hydrogen-resistant 2¼Cr1Mo-steels. … 2,25% Cr, 1% Mo  1.7015, …
  6. … hand welding. Excellent against pitting and stress corrosion. The PREN above 35 weldmetal offers outstanding resistance against pitting. …
  7. … in thick highly restrained weldments, since the possibility of premature service failure by intergranular HAZ cracking is reduced by …
  8. … free from porosity even on old and or otherwise diluted base material. Preheating is normally done to slow down the cooling speed, in case you …
  9. … cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding  … Cast aluminium special repairs, …
  10. Brand: Kobelco
    CEWELD Product: AA NiCro 625