1. … Stainless steel alloy for joining and cladding 17% Chromium alloys and …
  2. … of up to 450ºC. The recommended preheat temperature is 200ºC - 300°C unless the base material requires a higher preheat temperature. Use DC+ …
  3. … of titanium with carbon maintains a low level of free carbon and enables the filler metal to be used with Nickel 201. The weld metal has … of filler metal NiTi 3 include joining Nickel 200 and 201 to stainless steels, copper-nickel alloys, and Monel alloys. It is also used …
  4. … A high basic electrode for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% Mo types. CEWELD® 4462 Kb has high … variety of applications across all industrial segments.  … Duplex stainless steels,  1.4462, 1.4417, 1.4582, 1.4463, 1.4460, 1.4362, 1.4583, …
  5. … TIG rod with 2.25% Cr and 1% Mo content, with low carbon content (less than 0.05%), to be used for welding creep resistant steels. … For …
  6. … FL 830 ESHC is a highly basic flux for stainless steel strip electro slag cladding. Basicity: about 4,0 (according … Current: DC + Grain size: 2-16 … Electro slag (ESW) cladding with stainless steel strip, 308L, 309L, 316L, 2209 Duplex, 347, 309LNb, 309LMo. … …
  7. … CEWELD® AA R690 was one of “The first seamless rutile FCW with extreme low hydrogen for S690” Excellent for use … Weldox 700, Dillimax 690, Hardox, Naxtra 63, Naxtra 70, Optim 700 mc plus, Weldox 500, Hardox, Domex 460 MC, Domex 500 MC, Domex 550 MC, …
  8. … preponderantly spherical Coating microhardness: 800-1300 HV0.3 Sales units: Particle size* (DIN EN 1274 3.3): -45+22 μm (*other sizes on … ball valves, hydraulic rods, slush pump piston rods, corrugating rolles, hydroturbine buckes, hardchrome replacement. … Powder …
  9. … up-to 550 °C. The weld deposit of CEWELD DUR SS 60Ti is more or less comparable with HSS (High Speed Steel) and will offer outstanding …
  10. … tungsten to give improved long term creep properties. These consumables are specifically intended for high integrity structural service at …