1. … for economic welding of CrMoV-steels up to 550 °C. Due to the seamless production process the hydrogen content is below 3ml/100g weld …
  2. … of up to 450ºC. The recommended preheat temperature is 200ºC - 300°C unless the base material requires a higher preheat temperature. Use DC+ …
  3. … is only machinable by grinding. Due to the production method (seamless wire) this wire can be stored for a long time without the risk of …
  4. … FL 830 ESHC is a highly basic flux for stainless steel strip electro slag cladding. Basicity: about 4,0 (according … Current: DC + Grain size: 2-16 … Electro slag (ESW) cladding with stainless steel strip, 308L, 309L, 316L, 2209 Duplex, 347, 309LNb, 309LMo. … …
  5. … is only machinable by grinding. Due to the production method (seamless copper coated flux cored wire) this wire can be stored for a long …
  6. … Austenitic, non magnetic stainless steel alloy with high mechanical properties and excellent …
  7. … metals of similar composition to itself or to other grades of stainless steel. ER383 contains a low maximum of carbon, silicon, and sulfur …
  8. … up-to 550 °C. The weld deposit of CEWELD DUR SS 60Ti is more or less comparable with HSS (High Speed Steel) and will offer outstanding …
  9. … 16,000 hours. Suitable for joining and cladding Nickel alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy HX, X, Nickel alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy X …
  10. … wires with better arc stability and improved wetting properties with less spatters. Excellent results are also achieved without protective …