1. … Excellent welding properties and self detaching slag. The weld deposit can be …
  2. … The Ceweld AA 904LP is used for welding materials of similar chemical composition which are used for …
  3. … Designed for welding heat resistant steels to sustain working temperatures upto 650 …
  4. … recovery of 200%. For joining and surfacing in mechanical engineering, body and wagon building as well as in the fabrication of vessels and …
  5. … Without slag. Extremely crack resistant. Suitable for economic welding of CrMoV-steels up to 550 °C. Due to the seamless production …
  6. … with very good modelling properties, therefore excellent all-position welding with higher currents. Applicable down to -40°C. Low spatter …
  7. … treatable. Thicker sections should be preheated (150°C) prior to welding. … AlMgSi 0, AlSiMg (A), AlSi 1 MgMn, AlMg1SiCu, 3.3206, …
  8. … Submerged arc welding wire for high temperature creep resistant 2,45%Cr 1,0%Mo …
  9. … Special alloyed copper wire for Mig and Tig welding.       The weld metal is a Cu-Al bronze with high aluminium …
  10. … Heavy parts and thicker plates should be preheated (150°C), prior to welding. At the same time, it keeps the benefits of being relatively …