1. CEWELD ER80S-D2 Tig is a copper coated welding wire for welding of high strength steels, used predominantly after stress relieving. May find its use for joining … P295GH, P355GH, 16Mo3, 18MnMo4-5, 20MnMoNi4-5, P275NH, P355NH, P460NH, P355QH, P460QH, P500QH, GS-17CrMo55, GS-22CrMo5, GS-22CrMoV32, …
  2. … Like other nickel alloys, it is ductile, easy to form and weld, and possesses exceptional resistance to … exhibits outstanding resistance to pitting and crevice attack in the presence of chlorides and other halides. … Alloy C-2000, 2.4675, …
  3. … Hardfacing alloy for cladding steel mill rollers, thermoshock resistant and suitable for Francis and Pelton turbines. Used in … hardness and is resistant against metal-metal wear and high surface pressure.  … 1.4317, 1.4313, 1.4407, 1.4414,    GX4CrNi13-4, …
  4. CEWELD E FeNi 60 N has a few benefits compare to other “FeNi” types … current, non conductive coating and a powerful arc at very low amps. Preheating is normally done to slow down the cooling speed, in case you … EN-GJS-400-15, EN-GJS-400-18, EN-GJS-450-10, EN-GJS-500-7, EN-GJS-600-3, EN-GJS-700-2. GGG40, GGG45, GGG50, GGG60; GGG70, GGG80 … E FeNi …
  5. … point and narrow freezing range. In addition, it has a higher silicon content than AlSi5, which provides increased fluidity and reduced … elevated temperatures. Non-heat treatable. Thicker sections should be preheated (150°C) prior to welding. … G-AlSi10Mg, G-AlSi11, G-AlSi12 …
  6. … fiers de la qualité de nos produits, une norme qui est respectée par des tests rigoureux et des mesures de contrôle de qualité précises. Notre vaste gamme d’équipements de test de pointe témoigne de …
  7. Brand: Böhler Welding
    CEWELD Product: AA R690
    … - 60°C 47 J … 235 … diamondspark 700 RC
  8. … The weld metal of the CEWELD 35-45Nb can be used in a low-sulphur, carbon-enriching atmosphere up to 1175°C … resistance and good resistance to carburization and oxidation. No preheating or post heat treatment is necessary. Pay attention to low …
  9. … with niobium and titanium gives it the advantages of both these ferritic structure stabilizers: Titanium minimizes grain growth in Weld Metal zones (WM) due to titanium nitride (TiN) precipitation in the still liquid metal in these zones, thus avoiding …
  10. … This alloy offers excellent weldability when properly cleaned prior to welding. Heavy parts and thicker plates should be preheated (150°C), prior to welding The alloy shows good … 3.3315, 3.3535, 3.3206, 3.3541, EN AW 5005A, EN AW 5754, EN AW 6060, EN AC 51100, EN AW 5454, EN AW 5251,   … AlMg 3 … A 5.10: ER5754 …