1. … CEWELD 308H has been developed for typical operating temperatures up to 400ºC, and up to 600ºC in the short-term range. It also shows good … AISI 304, 304H, 312, 321H, 347, 347H,  UNS S30409, S32109, S34709, S30400, S32100, S34700 … 308H … A 5.9: ER308H … 14343-A: G 19 9 H …
  2. … and suitable for applications when exposed to hydrogen sulfide or sulfur dioxide. … The nominal composition (wt.-%) of filler metal of this …
  3. … and tempertures. It also withstands hydrogen chloride, sulfuric, acetic, hydrofluoric nd phosphoric acids. The alloy has improved …
  4. … 308H Tig has been developed for typical operating temperatures up to 400ºC, and up to 600ºC in the short-term range. It also shows good … AISI 304, 304H, 312, 321H, 347, 347H,  UNS S30409, S32109, S34709, S30400, S32100, S34700 … 308H Tig … A 5.9: ER308H … 14343-A: W 19 9 H …
  5. … as the base metal. Age hardened condition: 720ºC for 8 Hours, furnace Cool 55ºC/hour to 620ºC than Air Cool for 8 hours … Inconel …
  6. … than AISI 316 due to the high Mo. content. Suitable for use up to 400°C … 1.4429, 1.4434, 1.4435, 1.4436, 1.4438, 1.4439, 1.4453, …
  7. … high temperature corrosion, also in fuel-ash atmosphere containing sulfur and vanadium … ASTM B163, B166, B167, B168 with UNS N06690, IN657, …
  8. … and a Ni-based alloy. Crushed cast carbide will guaranty a long life. Furthermore the Ni-based alloy provides an excellent corrosion …
  9. … CEWELD® 320 Tig was designed specifically to withstand sulfuric acid. Its nickel, chromium, molybdenum and copper levels all …
  10. … good ductility after prolonged exposure at temperatures of 1200, 1400, 1600F (650, 760 and 870°C) for 16,000 hours. … Alloy HX, X, Nickel …