1. … in chloride-bearing solutions (a form of degradation to which the austenitic stainless steels are prone). It is able to withstand a wide range …
  2. … Preheating and interpass temperature 400-450 °C (austenitic welding) or 250-300 °C (martensitic welding). Root passes should …
  3. … A continuous, solid, corrosion-resistant, duplex wire for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% Mo types. …
  4. … NiCrMo 686 (UNS N06686/W.Nr. 2.4606) is a single-phase, austenitic Ni-Cr-Mo-W alloy offering outstanding corrosion-resistance in a … than competitive materials. … Duplex, super-duplex and super-austenitic stainless steels, nickel alloys such as UNS N06059 and N06022, …
  5. … Excelent weldabillity with fully austenitic weld metal with high resistance against stress corrosion cracking …
  6. … Fully austenitic weld metal with high resistance against stress corrosion cracking …
  7. … in chloride-bearing solutions (a form of degradation to which the austenitic stainless steels are prone).It is able to withstand a wide range …
  8. … Austenitic deposit with strain hardening properties and no limmits in the …
  9. … A high basic electrode for welding austenitic-ferritic stainless alloys of the 22% Cr, 5% Ni, 3% Mo …
  10. … High wear resistance and austenitic structure deposits. The deposit gives already a very good …