1. … Good resistance against hot cracking due to the high Mo content. During build-up welding, the weld metal already achieves approximately … 316LN, 316H, 316, 316Ti, 316Cb, 316LN, 444 S31640, S31603, S31653, S31600, S31630, S44400 … 309LMo Tig … A 5.9: ER309LMo … 14343-A: W 23 12 2 …
  2. … third parties that enables you to use only one wire to cover more procedures up to 460 MPa yield strength steels. CEWELD AA M460 can also be …
  3. … "NiLo'" and offer the lowest schrinkage possible to avoid cracks during heating and the cooling period. The weld deposit also retains … EN-GJS-400-15, EN-GJS-400-18, EN-GJS-450-10, EN-GJS-500-7, EN-GJS-600-3, EN-GJS-700-2. GGG40, GGG45, GGG50, GGG60; GGG70, GGG80 … AA …
  4. … root of the weld on the first pass and blankets the solidified weld during subsequent passes until the root surface temperature stays below 600 degrees F. Backup shielding also should be used on the back surface …
  5. … ductility after prolonged exposure at temperatures of 1200, 1400, 1600F (650, 760 and 870°C) for 16,000 hours. … Alloy HX, X, Nickel … Alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy X … A 5.14: ERNiCrMo-2 … 18274: S Ni 6002(NiCr21Fe18Mo9) …
  6. … de soudage et pour le développement de nouveaux procédés et procédures de soudage innovants. L'emplacement (600 m2) accueille les procédés de soudage innovants et de la plus haute …
  7. … souhaitez utiliser pour vos applications de rechargement. Avec une dureté de plus de 2400 HV et une surface extrêmement rugueuse, des … la buse de gaz (trailing) où les particules font partie du bain de soudure en cours de solidification. Lors de la journée thématique …
  8. … ductility after prolonged exposure at temperatures of 1200, 1400, 1600°F (650, 760 and 870°C) for 16,000 hours. Suitable for joining and … alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy HX, X, Nickel alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy X Tig … A 5.14: ERNiCrMo-2 … 18274: S Ni …
  9. … Tous nos fils de soudure sans soudure avec flux subissent un test complet 3.1 sur tous les métaux de soudure conformément à la norme EN 1597. En outre, la teneur en hydrogène …
  10. Brand: FILEUR
    … 40 … FILEUR DUR 404 M …