1. … arc stability with fast freezing slag. All quality values are dependent on compliance with the correct t8/5 time … Reh < 690 MPa Iso …
  2. … Recommended for operating temperatures up to 1150° C in carburized …
  3. … In this  Situation Ceweld SP NiAl is recommended. Suited for wear parts subject to extreme heavy abrasion …
  4. … welding speed with corresponding flux.  Suitable fluxes are depending on the weld metal requirements, in most cases CEWELD® FL 155 …
  5. … layer. A buffer layer with CEWELD® OA 4370 or CEWELD® OA MnCr is recommended in case of sensible base material or old layers. Weldable without …
  6. … In this  Situation Ceweld SP NiAl is recommended. Suited for wear parts subject to extreme heavy abrasion …
  7. … Ti can be used for a working temperature of up to 450ºC. The recommended preheat temperature is 200ºC - 300°C unless the base material …
  8. … (internal shielding gas). As they produce a slag, they are not recommended for multi-pass welding. … ISO 15608: 8.1 / TüV Groupe 29 (+22+21) …
  9. … The temperature limits for use under intermittent oxidation depend on cycle frequency. In no case shall a temperature of 1000°C be …
  10. … in the first layer. A buffer layer with OA 4370 or OA MnCr is recommended in case of sensible basematerial or old Hardface-layers. … 59-62 …