1. … / Solidus: 221°C / Liquidus: 279°C / Deposit color: Silver / Shear Strength (copper lap joint): 10,600 PSI … Copper, stainless steel … …
  2. … coated electrode for welding low alloyed steels with tensile strength up to 510 N/mm2. Recommended for root welding in pipelines due …
  3. … Multi-layer deposits are not recommended due to the extreme high hardness. Fused tungsten carbide will guaranty a long life for several …
  4. … Excelent corrosion resistance combined with high strength due to the addition of copper. The filler metal shows …
  5. … with abrasion. The martensitic structure gives this alloy good hot strength and oxidation resistance up to about 800 °C. Excellent rolling …
  6. … for the economic joining of fine grain structural steels with yield strength of Rp0,2 550 MPa (80 ksi). As welding flux we recommend our …
  7. … Excellent mechanical strength and welding properties due to a increased manganese and …
  8. … High   strength   Manganese-Molybdenum-  alloyed filler metal for flame …
  9. … by special carbide tools, hardening is possible. The maximum hardness is dependent on the base metal and is achieved in the first …
  10. … to most materials and requires minimal surface preparation. Bond strengths in excess of 9000 psi can be achieved on grit blasted …