1. … The 9%Cr-1%Mo creep resistant alloy is used for service up to ~600°C particularly in environments involving hot hydrogen gas. Flux …
  2. … and by grinding. The hardness of the weld deposit will degrees 20% at 600 °C and has a nominal hardness of 49-53 HRc at room temperature. The …
  3. … alloy offers superior wear protection, retaining its hardness up to 600ºC (1000ºF) with significant resistance to oxidation. … Aircraft gas …
  4. … for creep resistant service for working temperatures up to 600º C.  … 2,25% Cr, 1% Mo  1.7015, 1.7131, 1.7147, 1.7380, 1.7337, …
  5. … SAW welding stainless steels and Nickel based alloys: AISI 2205, Alloy 625, 904L Basicity: About 1,7 (according to Boniszewski) Current: DC or …
  6. … alloy offers superior wear protection, retaining its hardness up to 600ºC (1000ºF) with significant resistance to oxidation. … Aircraft gas …
  7. … is generally comparable to that of Rene 41 and generally superior to Inconel 718. Age hardenable while maintaining excellent … oxidation, at service temperatures ranging from 1200°F (650°C) up to 1600°F (870°C) … AMS 5708, 5709, 5706, 5707, 5704, 5544, 5586. PWA 1005, …
  8. … ductility after prolonged exposure at temperatures of 1200, 1400, 1600F (650, 760 and 870°C) for 16,000 hours. … Alloy HX, X, Nickel … Alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy X … A 5.14: ERNiCrMo-2 … 18274: S Ni 6002(NiCr21Fe18Mo9) …
  9. … ductility after prolonged exposure at temperatures of 1200, 1400, 1600°F (650, 760 and 870°C) for 16,000 hours. Suitable for joining and … alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy HX, X, Nickel alloys, stainless steel, carbon steel and low alloyed steels. UNS: N06002 … Alloy X Tig … A 5.14: ERNiCrMo-2 … 18274: S Ni …
  10. … based welding wires that are covered in AWS A 5.14 such as alloy 82, Inconel 600, 625, 601, 825, C276, alloy 59 etc. Basicity: about 3,3 (according to …