1. … Titanium carbides. The choice for the buffer layer is depending on the base metal and not always necessary.  … HRc 54-59, hardfacing alloy for …
  2. … Rutile Fe, Cr, Co and Mo based elektotrode with high hot wear resistance, tensile strenght and a …
  3. … layer with OA 4370 or OA MnCr is recommended in case of sensible base material or old layers. Weldable without protective gas. … Cement …
  4. … < 1,2% C ( Kohlenstoff). Weitere Legierungsbestandteile, insbesondere Nickel, Molybdän, Titan und Niob, verbessern die …
  5. … corrosion-resistance in a range of severe environments. Its high nickel (Ni) and molybdenum (Mo) provide good resistance in reducing … … Duplex, super-duplex and super-austenitic stainless steels, nickel alloys such as UNS N06059 and N06022, INCONEL alloy C-276, and …
  6. … rate and excellent weldability without slag losses. For critical base material or old hard facing layers it is necessary to buffer with …
  7. … without any risk of braking out or chipping of. In case of sensitive base material preheating is recommended at 300 - 400 °C. Old Hardfacing …
  8. … layer with OA 4370 or OA MnCr is recommended in case of sensible base material or old hardface-layers. Weldable without protective gas. …
  9. … or CEWELD® OA MnCr is recommended in case of old layers or critical base metals.. … 62-66 HRc Hardfacing alloy used in mining, agriculture …
  10. … Silicon bronze • Sound, pore free deposits on ferrous and non-ferrous base materials • Excellent corrosion resistance  … Welding thin steel …