1. … Cladding on low alloyed steels in case a 18/8/2 (AISI 316) CrNiMo layer is required in the first layer. … Strip cladding on low alloyed steels in case a 18/8/2 CrNiMo (AISI 316) layer is required in the first layer.  W.Nr: 1.4401, 1.4404, …
  2. … and excellent weldability, corrosion resistance is better than AISI 316 due to the high Mo. content and also offers excellent corrosion … X2CrNiMoN18-12-4, X2CrNiMo18-14-3, X3CrNiMnMoN19-16 UNS S31600, S31653, S31703, S31726, S31753 AISI 316Cb, 316L, 316LN, 317L, 317LN, …
  3. … slag fluxes. Cladding on low alloyed steels in case a 18/8/2 (AISI 316) CrNiMo layer is required in the first layer. … ISO 15608: 8.1 … 17 12 2, X6CrNiMoNb 17 12 3, X2CrNiMoN 17 12 3 (TP), X2CrMoTi18-2 316Cb, 316L, 316L, 316LN, 316H, 316, 316Ti, 316Cb, 316LN, 444 S31640, S31603, …
  4. Brand: ITW Elga - Hobart
    … Upon request Ceweld 4316 H … 43 … Cromarod 308 H …
  5. … where Molybdenum % is reduced to form a hybrid alloy between 308H and 316H, operates in temperatures up to 800 °C. CEWELD® 16.8.2-17 gives a … X8CrNiTi18-10, X8CrNiNb16-13, X6CrNiMoB17-12-2, 304H, 321H , 347H,  316H,  UNS 30409, S32109,S34709, S31609, 304S51, 321S51, 347S51, 316S51, 316S53  … 16.8.2-17 … A 5.4: ~E …
  6. Brand: Selectarc
    CEWELD Product: 316LMn
    … Existe en TIG … 52 … SELECTARC 20/10MN …
  7. … important steps to prevent hydrogen induced cracking are: 1)  Use airtight packing for covered electrodes 2)  Use seamless fluxcored wires …
  8. … cycling conditions up to 1200°C and carburized medias. Excellent fatigue strength and creep properties. … Cladding against high …
  9. … This alloy is often chosen to solve SCC problems, which may occur with 316L stainless … 2.4660, AISI 320 UNS N08020 Alloy 20, Carpenter 20, …
  10. Brand: Selectarc
    CEWELD Product: ER 80S-D2
    … Existe en TIG … 52 … SELECTARC F60 …